| Influence of MgO content on solidified electrolytic manganese residue with MgO and microbe |
| CHEN Zhe1,2,FANG Xiangwei1,2,LIU Hanlong1,2,LONG Kaiquan1,2,SHEN Chunni3 |
| (1. School of Civil Engineering,Chongqing University,Chongqing 400045,China;2. Key Laboratory of New Technology for Construction of Cities in Mountain Area,Ministry of Education,Chongqing University,Chongqing 400045,China;3. School
of Civil Engineering and Architecture,Chongqing University of Science and Technology,Chongqing 401331,China) |
|
|
|
|
Abstract As industrial waste,electrolytic manganese residue (EMR) has small particle size and poor permeability,so traditional microbial mineralization technology has great limitations in the treatment of the EMR. In this paper,the curing technology with MgO and microbe is proposed,the EMR in Xiushan Chongqing was treated by active MgO and microbe,the principle of curing tailing sand with MgO and microbe was discussed,the effects of active MgO content on water content,unconfined compressive strength,acid-base,XRD pattern and microstructure of solidified samples were studied. The research results indicate that the active MgO reacts with water,fills the micropores of the EMR,and carbonizes with in the air,the strength of solidified samples was improved to a certain extent,and under the action of bacteria,urea was hydrolyzed to form ,which rapidly carbonized the hydration products and further improved the strength of solidified samples. The higher the content of active MgO,the lower the moisture content,the higher the unconfined compressive strength and the higher the pH value of solidified sample of the EMR. The main products of curing tailing sand with MgO and microbe are nesquehonite,dypingite and hydromagnesite. The larger the content of active MgO,the higher the content of nesquehonite.
|
|
|
|
|
|
| [1] 中华人民共和国生态环境部. 中华人民共和国生态环境部2019年全国大、 中城市固体废物污染环境防治年报[R]. 北京:中华人民共和国生态环境部,2019.(Ministry of Ecology and Environment of the People?s Republic of China. Annual report on prevention and control of environmental pollution by solid waste in large and medium-sized cities in 2019[R]. Beijing:Ministry of Ecology and Environment of the People?s Republic of China,2019.(in Chinese))
[2] WHIFFIN V S. Microbial CaCO3 precipitation for the production of biocement[Ph. D. Thesis][D]. Murdoch:Murdoch University,2004.
[3] DEJONG J T,FRITZGES M B,NUSSLEIN K. Microbially induced cementation to control sand response to undrained shear[J]. Journal of Geotechnical and Geoenvironmental Engineering,2006,132(11):1 381–1 392.
[4] DEJONG J T,MORTENSEN B M,MARTINEZ B C,et al. Bio-mediated soil improvement[J]. Ecological Engineering,2010,36(2):197–210.
[5] 方祥位,申春妮,楚 剑,等. 微生物沉积碳酸钙固化珊瑚砂的试验研究[J]. 岩土力学,2015,36(10):2 773–2 779.(FANG Xiangwei,SHEN Chunni,CHU Jian,et al. An experimental study of coral sand enhanced through microbially-induced precipitation of calcium carbonate[J]. Rock and Soil Mechanics,2015,36(10): 2 773–2 779.(in Chinese))
[6] 谢约翰,唐朝生,尹黎阳,等. 纤维加筋微生物固化砂土的力学特性[J]. 岩土工程学报,2019,41(4):675–682.(XIE Yuehan,TANG Chaosheng,YIN Liyang,et al. Mechanical behavior of microbial-induced calcite precipitation (MICP)-treated soil with fiber reinforcement[J]. Chinese Journal of Geotechnical Engineering,2019,41(4):675–682.(in Chinese))
[7] 许朝阳,张 莉. 微生物改性对粉土强度的影响[J],建筑科学,2009,25(5):45–48.(XU Zhaoyang,ZHANG Li. The effect of microbes on strength of silt[J]. Building Science,2009,25(5):45–48.(in Chinese))
[8] 邵光辉,尤 婷,赵志峰,等. 微生物注浆固化粉土的微观结构与作用机理[J]. 南京林业大学学报:自然科学版,2017,41(2):129–135.(SHAO Guanghui,YOU Ting,ZHAO Zhifeng,et al. Microstructure and mechanism of microbial cementation silt treated by bio-grouting[J]. Journal of Nanjing Forestry University:Natural Sciences,2017,41(2):129–135.(in Chinese))
[9] 彭 劼,温智力,刘志明,等. 微生物诱导碳酸钙沉积加固有机质黏土的试验研究[J]. 岩土工程学报,2019,41(4):733–740. (PENG Jie,WEN Zhili,LIU Zhiming,et al. Experimental research on MICP-treated organic clay[J]. Chinese Journal of Geotechnical Engineering,2019,41(4):733–740.(in Chinese))
[10] 刘士雨,俞 缙,曾伟龙,等. 微生物诱导碳酸钙沉淀修复三合土裂缝效果研究[J]. 岩石力学与工程学报,2020,39(1):191–204. (LIU Shiyu,YU Jin,ZENG Weilong,et al. Repair effect of tabia cracks with microbially induced carbonate precipitation[J]. Chinese Journal of Rock Mechanics and Engineering,2020,39(1):191–204.(in Chinese))
[11] 许燕波,钱春香,陆兆文. 微生物矿化修复重金属污染土壤[J]. 环境工程学报,2013,7(7):2 763–2 768.(XU Yanbo,QIAN Chunxiang,LU Zhaowen. Remediation of heavy metal contaminated soils by bacteria biomineralization[J]. Chinese Journal of Environmental Engineering,2013,7(7):2 763–2 768.(in Chinese))
[12] 许朝阳,杨 贺,黄建璋,等. 生物修复Cu2+,Pb2+污染土的稳定性[J]. 工业建筑,2018,48(7):33–37.(XU Zhaoyang,YANG He,HUANG Jianzhang,et al. Stability of bioremediated soil contaminated by Cu2+ or Pb2+[J]. Industrial Construction,2018,48(7):33–37.(in Chinese))
[13] LISK M,VANDEPERRE L J,Al-TABBAA A. Influence of carbonation on the properties of reactive magnesia cement-based
pressed masonry units[J]. Advances in Cement Research,2008,20(2),53–64.
[14] UNLUER A T. Enhancing the carbonation of MgO cement porous blocks through improved curing conditions[J]. Cement and Concrete Research,2014,59:55–65.
[15] YI Y,LISKA M,UNLUER C,et al. Carbonating magnesia for soil stabilization[J]. Canadian Geotechnical Journal,2013,50(8):899–905.
[16] 刘松玉,李 晨. 氧化镁活性对碳化固化效果影响研究[J]. 岩土工程学报,2015,37(1):148–155. (LIU Songyu,LI Chen. Influence of MgO activity on stabilization efficiency of carbonated mixing method[J]. Chinese Journal of Geotechnical Engineering,2015,37(1):148–155.(in Chinese))
[17] 蔡光华,刘松玉,曹菁菁. 活性氧化镁碳化加固粉土微观机理研究[J]. 土木工程学报,2017,50(5):105–113.(CAI Guanghua,LIU Songyu,CAO Jingjing. Research on micro-mechanism of carbonated reactive MgO-stabilized silt[J]. China Civil Engineering Journal,2017,50(5):105–113.(in Chinese))
[18] 刘松玉,曹菁菁,蔡光华. 活性氧化镁碳化固化粉质黏土微观机制[J]. 岩土力学,2018,39(5):1 543–1 552.(LIU Songyu,CAO Jingjing,CAI Guanghua. Microstructural mechanism of reactive magnesia carbonated and stabilized silty clays[J]. Rock and Soil Mechanics,2018,39(5):1 543–1 552.(in Chinese))
[19] 方祥位,方艺霏,杨 阳,等. 基于活性氧化镁微生物固化尾矿砂的方法及其产品[P]:中国:CN110204289A,2019–09–06. (FANG Xiangwei,FANG Yifei,YANG Yang,et al. Based on the method of microorganism curing tailing sand with active magnesium oxide and its products[P]:China:CN110204289A,2019–09–06.(in Chinese))
[20] 中华人民共和国行业标准编写组. YB/T 4019—2006 轻烧氧化镁化学活性测定方法[S]. 北京:中国标准出版社,2006.(The Professional Standards Compilation Group of People?s Republic of ChinaYB/T 4019—2006 Test methods for chemical activity of caustic burned magnesia[S]. Beijing:China Standard Press,2006.(in Chinese))
[21] LIANG C,MOHAMED A S,JIAN C. Soil bio-cementation using a new one-phase low-pH injection method[J]. Acta Geotechnica,2019,14(3):615–626.
[22] 刘汉龙,肖 鹏,肖 杨,等. 微生物岩土技术及其应用研究新进展[J]. 土木与环境工程学报,2019,41(1):1–14.(LIU Hanlong,XIAO Peng,XIAO Yang,et al. State-of-the-art review of biogeotechnology and its engineering applications[J]. Journal of Civil and Environmental Engineering,2019,41(1):1–14.(in Chinese))
|
|
|
|